Enhancement of magnetic-field-induced strain in Ni-Fe-Ga-Co heusler alloy

Enhancement of magnetic-field-induced strain in Ni-Fe-Ga-Co heusler alloy
复制标题

DOI:
10.1016/j.scriptamat.2005.08.009
复制
发表时间:
2005-12
期刊:
影响因子:
6
通讯作者:
H. Morito;K. Oikawa;A. Fujita;K. Fukamichi;R. Kainuma;K. Ishida
H. Morito;K. Oikawa;A. Fujita;K. Fukamichi;R. Kainuma;K. Ishida
中科院分区:
材料科学1区
文献类型:
--
作者:
H. Morito;K. Oikawa;A. Fujita;K. Fukamichi;R. Kainuma;K. Ishida

文献摘要

被引文献

相似文献

估算了具有7层(14M)结构的Ni_(51)Fe_(18)Ga_(27)Co_3马氏体相在300K时的孪晶界面迁移率和磁晶各向异性常数K。马氏体相在300K下表现出约0.7%的大的磁场诱导应变。
The mobility of the twin boundary and the magnetocrystalline anisotropy constant K at 300K in the martensite phase of Ni51Fe18Ga27Co3with a 7-layered (14M) structure are estimated. The martensite phase exhibits a large magnetic-field-induced strain of about 0.7% at 300K.