Compressibility of pyrochlore-type MgZrSi2O7 determined by in situ X-ray diffraction in a large-volume high pressure appa ratus

Compressibility of pyrochlore-type MgZrSi2O7 determined by in situ X-ray diffraction in a large-volume high pressure appa ratus
复制标题

大容量高压装置中原位 X 射线衍射测定烧绿石型 MgZrSi2O7 的压缩性

DOI:
10.1080/08957959.2012.750653
复制
发表时间:
2013
影响因子:
2
通讯作者:
et al.
et al.
中科院分区:
物理与天体物理4区
文献类型:
--
作者:
S. Zhai;et al.

文献摘要

相似文献

采用同步能量色散x射线衍射法,在多顶锤高压装置中,在室温下测量了高达24.3 GPa的焦绿石型mgzrsi2o7。使用内部金金属压力校准器计算压力。本研究未观察到相变。采用三阶Birch-Murnaghan状态方程拟合压力-体积数据。拟合得到体积v0 =802.8±0.2 Å3,等温体积模量kt =249±12 GPa,一阶压力导数k t =3.2±1.3。将k′s固定为4,则KTis为241.8±2.6 GPa。与锆酸盐或钛酸盐型焦绿石相比,mgzrsi2o7由于阳离子半径比(rMg,Zr/rSi)较大而表现出较小的可压缩性。
The pyrochlore-type MgZrSi2O7has been investigated byin situsynchrotron energy-dispersive X-ray diffraction measurements up 24.3 GPa at room temperature in a multianvil high pressure apparatus. The pressure has been calculated using an internal gold metal pressure calibrant. No phase transformation was observed in this study. A third-order Birch–Murnaghan equation of state was used to fit the pressure–volume data. The fitting gives a volume ofV0=802.8±0.2 Å3, an isothermal bulk modulus ofKT=249±12 GPa, and first pressure derivative ofK′T=3.2±1.3. IfK′Tis fixed as 4,KTis obtained as 241.8±2.6 GPa. Compared with zirconate or titanate pyrochlores, MgZrSi2O7shows a smaller compressibility due to a larger cation radii ratio (rMg,Zr/rSi).