Infrared Photoacoustic Spectra of Japanese Cedar (Cryptomeria japonica D. Don) Wood and Bark Heat-Treated at Temperatures Ranging from 200℃ to 1100℃
Infrared Photoacoustic Spectra of Japanese Cedar (Cryptomeria japonica D. Don) Wood and Bark Heat-Treated at Temperatures Ranging from 200℃ to 1100℃
复制标题
200℃~1100℃热处理的日本柳杉(Cryptomeria japonica D. Don)木材和树皮的红外光声光谱
DOI:
--
复制
发表时间:
2003
期刊:
影响因子:
--
通讯作者:
S. Yamauchi
中科院分区:
文献类型:
--
作者:
S. Yamauchi
Wood (xylem) and bark of Japanese cedar (Cryptomeria japonica D. Don) were pyrolyzed over a wide range of temperatures (200 - HOO°C) in a nitrogen atmosphere. The infrared spectra of the heat-treated samples were recorded by a photo acoustic method. The photo acoustic spectral contours of wood and bark were very similar, showing several noticeable changes of spectral features with increasing heat-treatment temperature (HTT). In particular, two drastic spectral changes occurred in the HTT ranges of 200-300 o e and 600-700°C. It was indicated that O-H and e-H bonds remain in Japanese cedar heat-treated to 600°C. No vibrational band attributable to atomic groups containing a or H atoms could be found in the spectra obtained at 700 0 e or more.