Preparation and electrical properties of Mn silicides by reaction of MnCl2 and Si powder

Preparation and electrical properties of Mn silicides by reaction of MnCl2 and Si powder
复制标题

DOI:
10.1016/j.phpro.2011.01.023
复制
发表时间:
2011
期刊:
Physics Procedia
影响因子:
--
通讯作者:
Junhua Hu;Caili Zhang;Wen Li;S. Guan;H. Tatsuoka
Junhua Hu;Caili Zhang;Wen Li;S. Guan;H. Tatsuoka
中科院分区:
其他
文献类型:
--
作者:
Junhua Hu;Caili Zhang;Wen Li;S. Guan;H. Tatsuoka

文献摘要

被引文献

相似文献

用硅粉与MnCl2水蒸气反应合成了锰硅化物。生长温度为400℃~500℃,用X射线衍射仪对所合成的硅化物粉末进行了表征。通过粉末反应,硅化温度可降低到400℃,在500℃加热36h时,HMS以优势生长为主,讨论了HMS的相演变过程,并与体相反应进行了比较。测试了硅化锰片的电学性能。
Mn-silicides have been synthesized by reaction between Si powder and MnCl2vapour. The growth temperature varied from 400 °C to 500 °C. The resultant silicides powders were characterized by X-ray diffraction (XRD). By powder reaction, the silicidation temperature can be decreased to 400 °C. The dominant growth of HMS was obtained at the heating temperature of 500 °C for 36 h. The phase evolution was discussed and compared with bulk reaction. The electrical properties of Mn silicides tablets were measured.