文献摘要

被引文献

相似文献

在较宽的变形速率范围内(1-125×10−4s−1),Fe-6.5wt%Si合金具有极低的变形速率敏感性,这是由于该合金在400℃变形时具有极低的变形速率敏感性。这一发现为制备Fe-6.5wt%Si合金提供了一条高效的途径,并为组织控制提供了指导。
Outstanding ductility of Fe-6.5 wt%Si alloy can be obtained in a wide deformation rate range (1–125×10−4s−1) due to the ultra-low deformation rate sensitivity of the columnar-grained alloy with <100> orientation deformed at 400 °C. This finding provides a high-efficiency approach to prepare Fe-6.5 wt%Si alloy and a guideline for microstructure control.