In vitro degradation behaviour of non-porous ultra-fine poly(glycolic acid)/poly(l-lactic acid) fibres and porous ultra-fine poly(glycolic acid) fibres

In vitro degradation behaviour of non-porous ultra-fine poly(glycolic acid)/poly(l-lactic acid) fibres and porous ultra-fine poly(glycolic acid) fibres
复制标题

DOI:
10.1016/j.polymdegradstab.2005.04.015
复制
发表时间:
2005-12
影响因子:
5.9
通讯作者:
Y. You;S. Lee;J. Youk;B. Min;S. -. Lee;W. Park
Y. You;S. Lee;J. Youk;B. Min;S. -. Lee;W. Park
中科院分区:
化学2区
文献类型:
--
作者:
Y. You;S. Lee;J. Youk;B. Min;S. -. Lee;W. Park

文献摘要

被引文献

相似文献

The in vitro degradation behaviour of non-porous ultra-fine poly(glycolic acid)/poly(l-lactic acid) (PGA/PLA) fibres and porous ultra-fine PGA fibres was investigated. The non-porous ultra-fine PGA/PLA fibres were prepared by electrospinning of a PGA/PLA solution in 1,1,1,3,3,3-hexafluoro-2-propanol and the porous ultra-fine PGA fibres were obtained from them via selective removal of PLA with chloroform. Since PLA has a lower degradation rate than PGA, the degradation rates of the ultra-fine PGA/PLA fibres decreased with increasing content of PLA. The porous ultra-fine PGA fibres were degraded in vitro in the order of non-porous PGA>P-PGA/PLA(90/10)>P-PGA/PLA(70/30)>P-PGA/PLA(50/50)>P-PGA/PLA(30/70) due to autocatalytic hydrolysis.