ANTI-BACTERIAL AND MECHANICAL-PROPERTIES OF RESTORATIVE MATERIALS COMBINED WITH CHLORHEXIDINES
ANTI-BACTERIAL AND MECHANICAL-PROPERTIES OF RESTORATIVE MATERIALS COMBINED WITH CHLORHEXIDINES
复制标题
DOI:
10.1111/j.1365-2842.1983.tb00133.x
复制
发表时间:
1983-01-01
影响因子:
2.9
通讯作者:
KERPER, S
中科院分区:
文献类型:
--
作者:
JEDRYCHOWSKI, JR;CAPUTO, AA;KERPER, S
Chorhexidine gluconate or chlorhexidine dihydrochloride were added to a composite resin and a glass ionomer restorative material in concentrations of 0,1,2,3,5, and 10% by weight. Antibacterial activity was measured by inhibition of growth ofS. viridans, S. pyogenes, S. mutans, L. acidophilus, and E. coli.for 4 days.Compressive, tensile, and restorative material‐enamel adhesive shear strength tests were performed. The addition of chlorhexidine gluconate or chlorhexidine dihydrochloride increased the antibacterial activity of the composite resin and the glass ionomer restorative material and changed the mechanical properties of the restorative materials. The addition of chlorhexidine dihydrochloride resulted in mechanical properties closest to controls.