Effects of aging on the characteristics of Nd:YAG nano-powders

Effects of aging on the characteristics of Nd:YAG nano-powders
复制标题

DOI:
10.1016/j.jallcom.2010.04.144
复制
发表时间:
2010-07
影响因子:
6.2
通讯作者:
Xiaoli Zhang;Duo Liu;Y. Sang;Hong Liu;Ji-yang Wang
Xiaoli Zhang;Duo Liu;Y. Sang;Hong Liu;Ji-yang Wang
中科院分区:
材料科学2区
文献类型:
--
作者:
Xiaoli Zhang;Duo Liu;Y. Sang;Hong Liu;Ji-yang Wang

文献摘要

被引文献

相似文献

采用微波辅助沉淀法(MAP),在1373K下煅烧2h,制备了均匀、细小的Nd:YAG(Nd:Y3Al5O12)纳米粉体。研究发现,陈化条件对Nd:YAG纳米粉体的物相、形貌和烧结性能有显著影响。结果表明,为了获得均匀、纯相的Nd:YAG纳米粉体,应在密闭环境中进行时效处理。在密闭容器中陈化6 d的前驱体所得Nd:YAG纳米粉体的烧结性较好,晶粒较细。将Nd:YAG纳米粉体在密闭容器中陈化6 d后,在2003K下真空烧结10 h,得到透光率为75%的透明Nd:YAG陶瓷颗粒。
We report here the synthesis of homogeneous and fine Nd:YAG (Nd:Y3Al5O12) nano-powders via the microwave-assisted precipitation (MAP) method followed by calcination at 1373K for 2h. We find that the phase, morphology, and sinterability of the Nd:YAG nano-powders are affected remarkably by the conditions of aging. It is confirmed that aging should be performed in enclosed environment in order to obtain uniform and pure phase Nd:YAG nano-powders. The Nd:YAG nano-powders obtained from the precursors aged in enclosed vessel for 6 days showed better sinterability and finer grains than those aged in air. Transparent Nd:YAG ceramic pellet was obtained by vacuum sintering at 2003K for 10h (a transmittance of 75%) from the Nd:YAG nano-powders aged in enclosed vessel for 6 days.