Influence of different preparation and dyeing processes on the physical strength of the Ingeo fibre component in an Ingeo fibre/ cotton blend. Part 2: Bleaching followed by dyeing with disperse and reactive dyes
Influence of different preparation and dyeing processes on the physical strength of the Ingeo fibre component in an Ingeo fibre/ cotton blend. Part 2: Bleaching followed by dyeing with disperse and reactive dyes
复制标题
DOI:
10.1111/j.1478-4408.2004.tb00205.x
复制
发表时间:
2004
影响因子:
1.8
通讯作者:
D. Phillips;J. Suesat;M. Wilding;D. Farrington;Sophocles Sandukas;Dan Sawyer;J. Bone;Steve Dervan
中科院分区:
文献类型:
--
作者:
D. Phillips;J. Suesat;M. Wilding;D. Farrington;Sophocles Sandukas;Dan Sawyer;J. Bone;Steve Dervan
A study has been conducted to examine the effect of different preparation and dyeing processes on the physical strength of the Ingeo fibre component of an Ingeo fibre/cotton blend. An alkaline scouring process (for the cotton), followed by a two-bath, two-stage dyeing process in which the Ingeo fibre underwent a simulated dyeing with disperse dyes, followed by the cotton being dyed with reactive dyes, caused minimal deterioration to the strength of the Ingeo fibre. However, it is considered that problems might arise if the Ingeo fibre was subjected to prolonged dyeing times, particularly at neutral or alkaline pH, e.g. if an excessive number of shading additions needed to be carried out.