Takahara, Izumi;Shibata, Takayuki;Moritomo, Yutaka

文献摘要

被引文献

相似文献

三次电池是利用阳极和阴极材料之间的氧化还原电位(V)的热系数(α =dV/dT)之差(Δ α),通过环境热而不是电能充电。在原型NaxCo[Fe(CN)(6)](0.71)(NCF 71)/NaxCo[Fe(CN)(6)](0.90)(NCF 90)三次电池中,热循环性不好。这里,我们使用Ni取代的NaxNi[Fe(CN)(6)](0.68)(NNF 68)显著改善了三次电池的热循环性。Ni取代的NNF 68/NCF 90三次电池表现出良好的热循环性能:电池电压和容量在第10次热循环之前基本保持不变。
Tertiary battery is charged by the environmental heat, not by the electric energy, by using the difference (Delta alpha) in the thermal coefficient (alpha=dV/dT) of redox potential (V) between the anode and cathode materials. The thermal cyclability is not good in the prototypical NaxCo[Fe(CN)(6)](0.71) (NCF71)/NaxCo[Fe(CN)(6)](0.90) (NCF90) tertiary battery. Here, we significantly improved the thermal cyclability of the tertiary battery with using Ni-substituted NaxNi[Fe(CN)(6)](0.68) (NNF68). The Ni-substituted NNF68/NCF90 tertiary battery shows good thermal cyclability: both the cell voltage and capacity essentially unchanged up to the 10th thermal cycles.