Preferred orientation of ZnO nanoparticles formed by post-thermal annealing zinc implanted silica

Preferred orientation of ZnO nanoparticles formed by post-thermal annealing zinc implanted silica
复制标题

热退火后锌注入二氧化硅形成的 ZnO 纳米颗粒的优选取向

DOI:
10.1016/s0038-1098(02)00006-6
复制
发表时间:
2002-01-01
影响因子:
2.1
通讯作者:
Henderson, DO
Henderson, DO
中科院分区:
物理与天体物理4区
文献类型:
--
作者:
Liu, YX;Liu, YC;Henderson, DO

文献摘要

被引文献

相似文献

High quality zinc oxide nanoparticles with (002) preferred orientation were prepared by post-thermal annealing zinc implanted silica at 700 degreesC using two methods. One method was annealing zinc implanted silica at 700 degreesC for 2 h in oxygen ambient; the other method was sequentially annealing zinc implanted silica at 700 degreesC in nitrogen and oxygen ambient for 1 h, respectively. X-ray diffraction (XRD), absorption and microphotoluminescence (micro-PL) results indicated that the latter method could create high quality ZnO nanoparticles with (002) preferred orientation and narrow size-distribution. X-ray photoelectron spectra (XPS) showed the formation of ZnO nanoparticles on a silica surface, where the ZnO nanoparticle content increased with increasing oxidation time in an oxygen environment. The processes of the transformation from Zn to ZnO are discussed. (C) 2002 Elsevier Science Ltd. All rights reserved.