Simultaneously improved mechanical properties and corrosion resistance of Mg-Li-Al alloy produced by severe plastic deformation

Simultaneously improved mechanical properties and corrosion resistance of Mg-Li-Al alloy produced by severe plastic deformation
复制标题

DOI:
10.1016/j.msea.2018.08.077
复制
发表时间:
2018-09-26
影响因子:
6.4
通讯作者:
Sato, Hiroyuki
Sato, Hiroyuki
中科院分区:
材料科学1区
文献类型:
--
作者:
Mineta, Takahiro;Sato, Hiroyuki

文献摘要

被引文献

相似文献

研究了剧烈塑性变形(SPD)法制备的LA143合金试样的力学性能和耐腐蚀性能。结果表明,SPD是同时提高LA143合金试样在3.5质量% NaCl水溶液中维氏硬度和耐蚀性的有效方法。
In this study, the mechanical properties and corrosion resistance of LA143 alloy specimens produced by severe plastic deformation (SPD) were investigated. It was found that SPD was an effective way to simultaneously improve the Vickers hardness and corrosion resistance of LA143 alloy specimens in 3.5 mass% NaCl aqueous solution.