F racture or loss of esthetic veneers from a multiunit fixed partial denture (FPD) is troublesome. A repair technique for this type of failure was described by Johnston et al.,’and various methods of making an overcasting have been reported. 2-11 When a prosthesis is repaired, a strong bond between the overcasting and the undercasting is desirable. A metal conditioner capable of improving the bond of resin to noble metal alloys was recently introduced. i2 Laboratory evaluation has demonstrated improved durability of the bond that can be obtained with noble met-