Effect of cavity configuration and aging on the bonding effectiveness of six adhesives to dentin

Effect of cavity configuration and aging on the bonding effectiveness of six adhesives to dentin
复制标题

DOI:
10.1016/j.dental.2004.01.003
复制
发表时间:
2005-02-01
期刊:
影响因子:
5
通讯作者:
Van Meerbeek, B
Van Meerbeek, B
中科院分区:
工程技术1区
文献类型:
--
作者:
Shirai, K;De Munck, J;Van Meerbeek, B

文献摘要

被引文献

相似文献

目的:本研究的目的是确定聚合收缩应力的影响可能对债券durability.Methods:粘接效果进行了评估,通过微拉伸粘接强度测试(muTBS)和电子显微镜。测定平坦牙本质表面和标准化腔中的muTBS(这在1天和1年水储存之后)。应用了代表所有当前类别的六种粘合剂:两种蚀刻和冲洗(OptiBond FL,Kerr; Scotchbond 1,3 M ESPE),两个自蚀刻(Clearfil SE Bond,Kuraray; Adper Prompt,3 M,ESPE)和两种玻璃离聚物(Fuji Bond LC,GC; Reactmer,Shofu)粘合剂。传统的3步蚀刻和冲洗粘合剂OptiBond FL最有效地粘合到牙本质,并且似乎对聚合收缩应力和水降解不敏感。两步自蚀刻粘合剂Clearfit SE Bond最接近这种上级粘合效果,并且在1年的水暴露后仅略微损失粘合强度。两步蚀刻和冲洗粘合剂Scotchbond 1和“强”一步自蚀刻粘合剂Adper Prompt对腔体结构和水老化效应非常敏感。两步树脂改性的玻璃离子粘合剂富士债券LC只遭受收缩应力,而不是从1年的水暴露。值得注意的是,尽管1天的muTBS非常低,但当在水中储存1年时,“温和”1步玻璃离子粘合剂Reactmer的明显可修复性也是显著的:简化的粘合程序不一定意味着改善的粘合性能,特别是在长时间内。(C)2004年牙科材料学院。由爱思唯尔有限公司出版。保留所有权利。
Objectives: The purpose of this study was to determine the effect polymerization contraction stress may have on bond durability.Methods: Bonding effectiveness was assessed by micro-tensile bond strength testing (muTBS) and electron microscopy. The muTBS to flat dentin surfaces and in standardized cavities was determined (this after 1 day as well as 1 year water storage). Six adhesives representing all current classes were applied: two etch-and-rinse (OptiBond FL, Kerr; Scotchbond 1, 3M ESPE), two self-etch (Clearfil SE Bond, Kuraray; Adper Prompt, 3M, ESPE) and two glass-ionomer (Fuji Bond LC, GC; Reactmer, Shofu) adhesives.Results: The conventional 3-step etch-and-rinse adhesive OptiBond FL bonded most effectively to dentin, and appeared insensitive to polymerization shrinkage stress and water degradation. The 2-step self-etch adhesive Clearfit SE Bond most closely approached this superior bonding effectiveness and only slightly lost bond strength after 1-year water exposure. The 2-step etch-and-rinse adhesive Scotchbond 1 and the 'strong' 1-step self-etch adhesive Adper Prompt appeared very sensitive to cavity configuration and water-aging effects. The 2-step resin-modified glass-ionomer adhesive Fuji Bond LC only suffered from shrinkage stress, but not from 1-year water-exposure. Remarkable also is the apparent repairability of the 'mild' 1-step glass-ionomer adhesive Reactmer when stored for 1 year in water, in spite of the very tow 1-day muTBS.Significance: Simplified bonding procedures do not necessarily imply improved bonding performance, especially in the tong term. (C) 2004 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.