Effect of pre-swelling of coal at mild temperatures on its hydro-liquefaction properties
Effect of pre-swelling of coal at mild temperatures on its hydro-liquefaction properties
复制标题
温和温度下煤预膨胀对其加氢液化性能的影响
DOI:
10.1016/j.fuproc.2009.03.022
复制
发表时间:
2009-07
影响因子:
7.5
通讯作者:
Wei, Xianyong
中科院分区:
文献类型:
--
作者:
Cao, Meixia;Shui, Hengfu;Wang, Zhicai;Liu, Jianlong;Wei, Xianyong
The effects of pre-swelling treatment of Shenhua coal at mild temperatures (less than 160 °C) on its hydro-liquefaction properties were determined in this paper. It was found that with the increase of pre-swelling temperature in tetralin (THN) up to 120 °C, the liquefaction conversions of swollen coals increased. However, when N-methyl-2-pyrrolidinone (NMP) was used as swelling solvent, the liquefaction conversion decreased with the increase of pre-swelling temperature. The liquefied product distributions were very much dependent on the pre-swelling pretreatment conditions, and the mechanism was discussed. Based on the results obtained, a new swelling-liquefaction combining technology (SLCT) was advanced, in which the liquefaction conversion and oil+gas yield were enhanced.
登录
查看更多内容
影响因子:
7.4
作者:
F. Derbyshire;A. Davis;M. Epstein;P. Stansberry
通讯作者:
F. Derbyshire;A. Davis;M. Epstein;P. Stansberry
影响因子:
5.3
作者:
Toshimitsu Suzuki
通讯作者:
Toshimitsu Suzuki
影响因子:
7.4
作者:
T. Takanohashi
通讯作者:
T. Takanohashi
影响因子:
5.3
作者:
S. Brandes;R. Graff;M. L. Gorbaty;M. Siskin
通讯作者:
S. Brandes;R. Graff;M. L. Gorbaty;M. Siskin
影响因子:
7.4
作者:
Shui, Hengfu;Wang, Gaoqiang;Wang, Zhicai
通讯作者:
Wang, Zhicai