Preparation and Morphologies of Shell Cross-Linked Micelles Based on Commercial Poly(styrene-block-ethylene-co-butene-block-styrene)

Preparation and Morphologies of Shell Cross-Linked Micelles Based on Commercial Poly(styrene-block-ethylene-co-butene-block-styrene)
复制标题

商业聚苯乙烯-嵌段-乙烯-共聚-丁烯-嵌段-苯乙烯壳交联胶束的制备及形貌

DOI:
--
复制
发表时间:
2002
期刊:
影响因子:
--
通讯作者:
M. Jiang
M. Jiang
中科院分区:
--
文献类型:
--
作者:
Tianlong Li;Fanglin Ning;Jingwei Xie;Daoyong Chen;M. Jiang

文献摘要

被引文献

相似文献

通过Friedel-Crafts反应将氯甲基引入氢化聚苯乙烯-嵌段-丁二烯-嵌段-苯乙烯(SEBS)的聚苯乙烯(PS)嵌段中。产物(SEBS-CH_2Cl)在THF/乙醇(10/9,v/v)中形成了以PS为冠、以氢化PB为核的球形胶束。然后,以1,6-己二胺为交联剂,通过胺化使带有CH 2Cl基团的聚苯乙烯电晕交联。壳交联胶束呈球形核壳结构,在溶液中是稳定的,这是通过DLS在溶液中和TEM在固态下验证。
Chloromethyl groups were introduced into the polystyrene (PS) blocks of hydrogenated poly(styrene-block-butadiene-block-styrene) (SEBS) via Friedel–Crafts reaction. The product (SEBS-CH2Cl) formed spherical micelles with PS corona and hydrogenated PB core in THF/ethanol (10/9, v/v). Then, the polystyrene corona carrying CH2Cl groups was cross-linked by amination with 1,6-hexanediamine as a cross linker. The shell cross-linked micelles showed spherical core-shell structure and were stable in solution, which was verified by DLS in solution and by TEM in the solid state.