Crystal growth and structure of R2Ir2O7 (R = Pr, Eu) using molten KF

Crystal growth and structure of R2Ir2O7 (R = Pr, Eu) using molten KF
复制标题

DOI:
10.1016/j.materresbull.2006.08.011
复制
发表时间:
2007-05-03
影响因子:
5.4
通讯作者:
Chan, Julia Y.
Chan, Julia Y.
中科院分区:
材料科学2区
文献类型:
--
作者:
Millican, Jasmine N.;Macaluso, Robin T.;Chan, Julia Y.

文献摘要

被引文献

相似文献

在1373 K下,用熔融KF法合成了R2Ir2O7(R = Pr,Eu)单晶。烧绿石化合物以立方空间群Fd(3)在巴m(No.227,原点选择2)上结晶,其中Z = 8。室温下,Pr_2Ir_2O_7和Eu_2Ir_2O_7的晶格常数分别为a = 10.3940(4)埃,V = 1122.92(7)埃和a = 10.274(3)埃,V = 1084.5(6)埃。本文报道了R_2Ir_2O_7(R. = Pr,Eu),并在110、115和298 K下用单晶X射线衍射实验测定了它们的结构。(c)2006爱思唯尔有限公司版权所有。
Single crystals of R2Ir2O7 (R = Pr, Eu) have been synthesized using molten KF at 1373 K. The pyrochlore compounds crystallize in a cubic space group Fd(3) over bar m (No. 227, origin choice 2), with Z = 8. At room temperature, the lattice parameters are a = 10.3940(4) angstrom, V = 1122.92(7) angstrom(3) and a = 10.274(3) angstrom, V = 1084.5(6) angstrom(3) for Pr2Ir2O7 and Eu2Ir2O7, respectively. In this paper, we report the crystal growth of R2Ir2O7 (R. = Pr, Eu) and their structure determinations from single crystal X-ray diffraction experiments at temperatures of 110, 115, and 298 K. (c) 2006 Elsevier Ltd. All rights reserved.