Dielectric Critical Slowing-Down in Ferroelectric (CH3NHCH2COOH)3·CaCl2
Dielectric Critical Slowing-Down in Ferroelectric (CH3NHCH2COOH)3·CaCl2
复制标题
铁电材料的介电临界减速 (CH3NHCH2COOH)3·CaCl2
DOI:
10.1143/jpsj.52.1897
复制
发表时间:
1983
影响因子:
1.7
通讯作者:
Kuninobu Tanaka
中科院分区:
文献类型:
--
作者:
K. Deguchi;Noriari Aramaki;E. Nakamura;Kuninobu Tanaka
Complex dielectric constants of (CH 3 NHCH 2 COOH) 3 ·CaCl 2 and (CH 3 NDCH 2 COOD) 3 ·CaCl 2 have been measured. between 10 4 Hz and 10 9 Hz in the Curie temperature region. No appreciable isotope effect was found in the complex dielectric constants as well as in the Curie temperature. Dielectric dispersion of the Debye type which showed a critical slowing-down was observed above about 100 MHz. Discussion was made of the relation between the observed critical slowing-down and the softening of the optical phonon reported previously.