Improvement of soft magnetic properties in (Fe0.85B0.15)100-xCux melt-spun alloys

Improvement of soft magnetic properties in (Fe0.85B0.15)100-xCux melt-spun alloys
复制标题

DOI:
10.2320/matertrans.maw200730
复制
发表时间:
2007-09-01
影响因子:
1.2
通讯作者:
Yoshizawa, Yoshihito
Yoshizawa, Yoshihito
中科院分区:
材料科学4区
文献类型:
--
作者:
Ohta, Motoki;Yoshizawa, Yoshihito

文献摘要

被引文献

相似文献

讨论了快淬法制备的(Fe0.85B0.15)(100-x)Cux合金退火后的铜含量对磁性能的影响。在x=1.0~1.5范围内,随着x的增加,H-c值显著减小,晶粒度显著减小。当x=1.5时,合金表现出良好的磁性能,小的H-c约为7A/m,高的B,大于1.8T。在本合金体系中,添加1.0%以上的铜有利于纳米晶的形成和软磁性能的改善。
The Cu content dependence of magnetic properties in annealed (Fe0.85B0.15)(100-x)Cu-x alloys fabricated by melt-spinning was discussed. The value of H-c markedly decreases with increasing x between x = 1.0 and 1.5, accompanied with significant reduction of crystalline grain size. The alloy with x = 1.5 showed excellent magnetic properties such as a small H-c of about 7 A/m and a high B, of more than 1.8 T. For the present alloy system, more than 1.0% addition of Cu is effective for the formation of nano-scale grains and for the improvement of the soft magnetic properties.