亚稳态四方KNbO 3 可以由层状钙钛矿K 2 NbO 3 F通过室温下的拓扑化学反应2-96小时合成。层状钙钛矿 K 2 NbO 3 F 中的岩盐型 KF 块选择性地溶解在水中,得到三维钙钛矿 KNbO 3 。这种转变具有拓扑特征,因为钙钛矿块被保留。
Metastable tetragonal KNbO 3 can be synthesized from the layered perovskite, K 2 NbO 3 F, via a topochemical reaction at room temperature for 2 - 96 h. The rock-salt type KF blocks in the layered perovskite, K 2 NbO 3 F, were selectively dissolved in water to give a three-dimensional perovskite, KNbO 3 . This transformation has a topotactic character because the perovskite block is preserved.