Electrochemical Reactivity of LiFePO4 Prepared by Hydrothermal Method

Electrochemical Reactivity of LiFePO4 Prepared by Hydrothermal Method
复制标题

DOI:
10.1246/cl.2006.338
复制
发表时间:
2006-02
期刊:
影响因子:
1.6
通讯作者:
DokkoKaoru;KoizumiShohei;KanamuraKiyoshi
DokkoKaoru;KoizumiShohei;KanamuraKiyoshi
中科院分区:
化学4区
文献类型:
--
作者:
DokkoKaoru;KoizumiShohei;KanamuraKiyoshi

文献摘要

被引文献

相似文献

以CH3COOLi、FeSO4和(NH4)2HPO4为原料,在170℃下,采用水热法制备LiFePO4。所得LiFePO4的粒径约为3 μm。LiFePO4作为po的性能…
LiFePO4 was prepared by hydrothermal method starting from CH3COOLi, FeSO4, and (NH4)2HPO4 at 170 °C. The particle size of the obtained LiFePO4 was about 3 μm. The performance of the LiFePO4 as a po...