Aqueous tape casting of 10 mol%-Gd 2O 3-doped CeO 2 nano-particles

Aqueous tape casting of 10 mol%-Gd 2O 3-doped CeO 2 nano-particles
复制标题

DOI:
10.1016/j.msea.2006.05.073
复制
发表时间:
2006-08
影响因子:
6.4
通讯作者:
L. Luo;A. Tok;F. Boey
L. Luo;A. Tok;F. Boey
中科院分区:
材料科学1区
文献类型:
--
作者:
L. Luo;A. Tok;F. Boey

文献摘要

被引文献

相似文献

The aqueous tape casting process was systematically developed and investigated for the tape casting of 10mol%-Gd2O3-doped CeO2nano-particles. This study focused on obtaining the optimum slurry formulations and on the effects of the processing parameters such as the stability, the rheology and the wetting properties on the tape characteristics. High solid loading (55vol.%) and stable slurries of 10GDC nano-particles were achieved using poly(acrylic acid) (PAA) as a dispersant; poly(vinyl alcohol) (PVA) as a binder; poly(ethylene glycol) (PEG) as a plasticizer; octanol as a defoamer and 2,4,7,9-tetramethyl-5-decyne-4,7-diol ethoxylate as a surfactant. The pH values of the slurries were maintained in the range of 9.0–10.0. Homogeneous, defect-free green tapes (thickness 150–200μm) with smooth surface and high relative green density (51.5%) were thus successfully obtained.