Hydrogen decrepitation of sintered NdFeB magnets

Hydrogen decrepitation of sintered NdFeB magnets
复制标题

DOI:
10.1109/20.312372
复制
发表时间:
1994-03
影响因子:
2.1
通讯作者:
C. Stiller;S. Roth;A. Binner
C. Stiller;S. Roth;A. Binner
中科院分区:
工程技术4区
文献类型:
--
作者:
C. Stiller;S. Roth;A. Binner

文献摘要

被引文献

相似文献

本文研究了NdFeB烧结磁体吸放氢的动力学行为。在高于200/spl deg/C的温度下的氢化用于破碎富Nd相。Nd/sub 2/Fe/sub 14/B相的晶粒没有受到损伤。氢解吸分几个阶段进行,并在约400/spl deg/C下完成。>
The kinetics of the hydrogen absorption and desorption behaviour of a NdFeB sintered magnet is studied. Hydrogenation at temperatures above 200/spl deg/C is used to crumble the Nd-enriched phase. The grains of Nd/sub 2/Fe/sub 14/B phase remain undamaged. Hydrogen desorption occurs in several stages and is complete at approximately 400/spl deg/C. >