采用铸造、熔融淬火和熔融纺丝三种方法制备了掺杂tb (Fe0.83Ga0.17)100−xTbx(0≤x≤0.47)。在fe83ga17合金中加入Tb固体,可显著提高合金的磁致伸缩性能。在(Fe0.83Ga0.17)99.77 tb0.23熔纺带中实现了高达- 886 ppm的巨大垂直磁致伸缩λ⊥。磁致伸缩的增强被认为与Tb掺杂fe83ga17合金引起的强局部磁晶各向异性有关。
Three methods, casting, melt-quenching and melt-spinning were applied for preparing Tb-doped (Fe0.83Ga0.17)100−xTbx(0 ⩽x ⩽0.47). The magnetostriction improved drastically by Tb solid dissolved in Fe83Ga17alloys. A giant perpendicular magnetostrictionsλ⊥up to −886 ppm was achieved in the (Fe0.83Ga0.17)99.77Tb0.23melt-spun ribbons. The enhanced magnetostriction was thought to be associated with the strong local magnetocrystalline anisotropy caused by the Tb doping into Fe83Ga17alloys.
掺 Tb Fe83Ga17 熔纺带材中的超磁致伸缩
DOI: 10.1063/1.4851216
发表时间: 2013-07
影响因子: 4
作者:
Wei Wu, Jinghua Liu, Chengbao Jiang, Huibin Xu
通讯作者: Wei Wu, Jinghua Liu, Chengbao Jiang, Huibin Xu
DOI: 10.1002/9781119562269.ch2
发表时间: 2020-11
期刊: Magnetic Memory Technology
影响因子: --
作者:
D. Tang;C. Pai
通讯作者: D. Tang;C. Pai
DOI: 10.1063/1.4809829
发表时间: 2013-06-03
影响因子: 4
作者:
Jiang, Liping;Yang, Jiandong;Harris, Vincent G.
通讯作者: Harris, Vincent G.
DOI: 10.1016/s1574-9304(05)80122-1
发表时间: 1980
期刊: Handbook of Ferromagnetic Materials
影响因子: --
作者:
A. Clark
通讯作者: A. Clark
DOI: 10.1063/1.3456502
发表时间: 2010-08
影响因子: 3.2
作者:
Jinghua Liu;Zhibin Wang;Chengbao Jiang;Huibin Xu
通讯作者: Jinghua Liu;Zhibin Wang;Chengbao Jiang;Huibin Xu