Oxidation of low-alloy steel in high temperature steam and supercritical water
Oxidation of low-alloy steel in high temperature steam and supercritical water
复制标题
DOI:
10.1080/09603409.2017.1286549
复制
发表时间:
2017-02
影响因子:
1.3
通讯作者:
Xu Hong
中科院分区:
文献类型:
--
作者:
Zhang Naiqiang;Yue Guoqiang;Lv Fabin;Zhu Zhongliang;Khan Hasan Izhar;Xu Hong
Abstract The oxidation behaviour of a low-alloy steel T22 was investigated by exposure to ordinary pressure steam (0.1 MPa), high-pressure superheated steam (8 MPa), and supercritical water (SCW) (25 MPa) at 600 °C for 1000 h. The results show the exposur
登录
查看更多内容
影响因子:
8.3
作者:
Martinelli, L.;Balbaud-Celerier, F.;Santarini, G.
通讯作者:
Santarini, G.
影响因子:
3.1
作者:
Bischoff, Jeremy;Motta, Arthur T.;Allen, Todd R.
通讯作者:
Allen, Todd R.
影响因子:
2.2
作者:
J. Zurek;M. Michalik;F. Schmitz;T. Kern;L. Singheiser;W. Quadakkers
通讯作者:
J. Zurek;M. Michalik;F. Schmitz;T. Kern;L. Singheiser;W. Quadakkers
影响因子:
6
作者:
Yamaguchi, T
通讯作者:
Yamaguchi, T
影响因子:
8.3
作者:
Ehlers, J.;Young, D. J.;Quadakkers, W. J.
通讯作者:
Quadakkers, W. J.