The more shearing, the thicker shear band and heat-affected zone in bulk metallic glass

The more shearing, the thicker shear band and heat-affected zone in bulk metallic glass
复制标题

剪切越多,块体金属玻璃的剪切带和热影响区越厚

DOI:
10.1557/jmr.2008.0258
复制
发表时间:
2008-08
影响因子:
2.7
通讯作者:
Guo, H.
Guo, H.
中科院分区:
材料科学4区
文献类型:
--
作者:
Zhang, Z.F.;Sui, M.L.;Xiao, N.M.;Wen, J.;Guo, H.

文献摘要

参考文献

被引文献

相似文献

在对一种锆基大块金属玻璃的压缩试验中,在圆柱形止动块断裂之前,保留了一条主要的剪切带。在变形样品的中心发现了厚度为10μm的热影响区,并伴有剪切带。
In a compression test for a Zr-based bulk metallic glass, a dominant shear band was preserved before fracture by a cylindrical stopper. A heat-affected zone (HAZ) ∼10 μm thick together with shear band was discovered in the center of the deformed sample by
DOI: 10.1557/jmr.2002.0214
发表时间: 2002-06-01
影响因子: 2.7
作者:
Hufnagel, TC;Jiao, T;Ramesh, KT
通讯作者: Ramesh, KT
DOI: 10.1007/s11661-998-0004-6
发表时间: 1998-07-01
影响因子: 2.8
作者:
Liu, CT;Heatherly, L;Inoue, A
通讯作者: Inoue, A
DOI: 10.1002/9781118801017.ch7.10
发表时间: 2021-02
期刊: Encyclopedia of Glass Science, Technology, History, and Culture
影响因子: --
作者:
D. V. Louzguine-Luzgin;A. Inoue
通讯作者: D. V. Louzguine-Luzgin;A. Inoue
DOI: 10.1126/science.1136726
发表时间: 2007-03-09
期刊: SCIENCE
影响因子: 56.9
作者:
Liu, Yan Hui;Wang, Gang;Wang, Wei Hua
通讯作者: Wang, Wei Hua
DOI: 10.1080/09500830701413904
发表时间: 2007-08
影响因子: 1.2
作者:
K. Mondal;G. Santhosh Kumar;T. Ohkubo;K. Oishi;T. Mukai;K. Hono
通讯作者: K. Mondal;G. Santhosh Kumar;T. Ohkubo;K. Oishi;T. Mukai;K. Hono