Apatite formation of substituted Bioglass 45S5: SBF vs. Tris

Apatite formation of substituted Bioglass 45S5: SBF vs. Tris
复制标题

替代 Bioglass 45S5 的磷灰石形成:SBF 与 Tris

DOI:
10.1016/j.matlet.2019.126760
复制
发表时间:
2019
期刊:
影响因子:
3
通讯作者:
DS Brauer
DS Brauer
中科院分区:
材料科学3区
文献类型:
--
作者:
R Wetzel;DS Brauer

文献摘要

参考文献

被引文献

相似文献

无细胞介质浸泡实验是表征生物活性玻璃离子释放和磷灰石沉淀的关键步骤。我们发现,与Tris-HCl缓冲液相比,生物玻璃45S5和其他两种玻璃的磷灰石形成在模拟体液(SBF)中被延迟,可能是由于SBF中的高镁浓度。此外,FTIR和XRD结果表明,SBF中形成的磷灰石由于较高的取代(如碳酸盐)而更加无序。2.5% Zn取代Ca可减少离子释放,而2.5% Mg取代Ca无此作用,但两种取代均可延缓磷灰石的形成。
Immersion experiments in acellular media are a key step in characterising bioactive glass ion release and apatite precipitation. We show that apatite formation of Bioglass 45S5 and two other glasses is delayed in simulated body fluid (SBF) compared to Tris-HCl buffer, likely owing to high magnesium concentrations in SBF. In addition, FTIR and XRD results suggest apatite formed in SBF to be more disordered owing to higher substitution (e.g. by carbonate). 2.5% Zn for Ca substitution reduced ion release, while 2.5% Mg for Ca substitution showed no such effect, but both substitutions delayed apatite formation in either medium.
DOI: 10.1111/ijag.12288
发表时间: 2017-12-01
影响因子: 2.1
作者:
Kirste, Gloria;Brandt-Slowik, Juliane;Brauer, Delia S.
通讯作者: Brauer, Delia S.
DOI: --
发表时间: 2002
期刊:
影响因子: --
作者:
A. Helebrant;L. Jonášová;L. Sanda
通讯作者: L. Sanda
合成碳酸羟基磷灰石中的锌离子。
DOI: 10.1016/0003-9969(94)90040-x
发表时间: 1994
影响因子: 3
作者:
I. Mayer;F. Apfelbaum;J. Featherstone
通讯作者: J. Featherstone
DOI: 10.1016/j.actbio.2012.08.051
发表时间: 2013-02-01
期刊: ACTA BIOMATERIALIA
影响因子: 9.7
作者:
Fagerlund, S.;Hupa, L.;Hupa, M.
通讯作者: Hupa, M.