Surface-Directed Mineralization of Fibrous Collagen Scaffolds in Simulated Body Fluid for Tissue Engineering Applications.

Surface-Directed Mineralization of Fibrous Collagen Scaffolds in Simulated Body Fluid for Tissue Engineering Applications.
复制标题

DOI:
10.1021/acsabm.0c01507
复制
发表时间:
2021-03-15
影响因子:
4.7
通讯作者:
Bedran-Russo AK
Bedran-Russo AK
中科院分区:
其他
文献类型:
--
作者:
Bim-Júnior O;Curylofo-Zotti F;Reis M;Alania Y;Lisboa-Filho PN;Bedran-Russo AK

文献摘要

参考文献

被引文献

相似文献

利用聚合物添加剂稳定流体无定形磷酸钙(ACP)是体外获得胶原纤维内矿化的关键。另一方面,这种仿生方法抑制了无约束的纤维外空间中矿物晶体的成核,即纤维外矿化。纤维外矿物质含量是硬结缔组织(如骨和牙本质)复制的一个重要特征,因为它有助于最终的微结构和生物矿物复合材料的机械刚度。在此,我们报告了一种直接的途径,通过无聚合物添加剂的表面导向工艺生产密集矿化胶原复合材料。模拟体液(1× SBF)被用作仿生结晶介质,在胶原蛋白表面进行预加载程序,快速生成启动基质矿化所需的无定形前体物质。这种方法可以在大量胶原蛋白支架中形成纤维外生物活性矿物质,这可能为组织工程和修复目的的骨导电性胶原-磷灰石材料的生产提供优势。
The use of polymer additives that stabilize fluidic amorphous calcium phosphate (ACP) is key to obtaining intrafibrillar mineralization of collagen in vitro. On the other hand, this biomimetic approach inhibits the nucleation of mineral crystals in unconfined extrafibrillar spaces, that is, extrafibrillar mineralization. The extrafibrillar mineral content is a significant feature to replicate from hard connective tissues such as bone and dentin as it contributes to the final microarchitecture and mechanical stiffness of the biomineral composite. Herein, we report a straightforward route to produce densely mineralized collagenous composites via a surface-directed process devoid of the aid of polymer additives. Simulated body fluid (1× SBF) is employed as a biomimetic crystalizing medium, following a preloading procedure on the collagen surface to quickly generate the amorphous precursor species required to initiate matrix mineralization. This approach consistently leads to the formation of extrafibrillar bioactive minerals in bulk collagen scaffolds, which may offer an advantage in the production of osteoconductive collagen–apatite materials for tissue engineering and repair purposes.
DOI: 10.1016/j.dental.2013.10.012
发表时间: 2014-01
期刊: DENTAL MATERIALS
影响因子: 5
作者:
Bedran-Russo, Ana K.;Pauli, Guido F.;Chen, Shao-Nong;McAlpine, James;Castellan, Carina S.;Phansalkar, Rasika S.;Aguiar, Thaiane R.;Vidal, Cristina M. P.;Napotilano, Jose G.;Nam, Joo-Won;Leme, Ariene A.
通讯作者: Leme, Ariene A.
在羟基磷灰石成核抑制剂存在下胶原蛋白在骨磷灰石形成中的作用。
DOI: 10.1038/nmat2875
发表时间: 2010-12
期刊: Nature materials
影响因子: 41.2
作者:
通讯作者: --
DOI: 10.1371/journal.pone.0029258
发表时间: 2012
期刊: PloS one
影响因子: 3.7
作者:
McNally EA;Schwarcz HP;Botton GA;Arsenault AL
通讯作者: Arsenault AL
DOI: 10.1021/cr800443h
发表时间: 2008-11
期刊: CHEMICAL REVIEWS
影响因子: 62.1
作者:
Gower, Laurie B.
通讯作者: Gower, Laurie B.
DOI: 10.1016/j.biomaterials.2009.01.008
发表时间: 2009-04-01
期刊: BIOMATERIALS
影响因子: 14
作者:
Bohner, Marc;Lemaitre, Jacques
通讯作者: Lemaitre, Jacques