Microstructural Evolution of Ni-Sn Transient Liquid Phase Sintering Bond during High-Temperature Aging
Microstructural Evolution of Ni-Sn Transient Liquid Phase Sintering Bond during High-Temperature Aging
复制标题
Ni-Sn瞬态液相烧结键高温时效过程中的微观结构演变
DOI:
10.1007/s11664-018-6336-0
复制
发表时间:
2018-05
影响因子:
2.1
通讯作者:
Zhao Xingke
中科院分区:
文献类型:
--
作者:
Feng Hongliang;Huang Jihua;Peng Xianwen;Lv Zhiwei;Wang Yue;Yang Jian;Chen Shuhai;Zhao Xingke
For high-temperature-resistant packaging of new generation power chip, a chip packaging simulation structure of Ni/Ni-Sn/Ni was bonded by a transient liquid-phase sintering process. High-temperature aging experiments were carried out to investigate joint
登录
查看更多内容
DOI:
10.2298/jmmb121123052o
发表时间:
2012
期刊:
Journal of Mining and Metallurgy, Section B
影响因子:
--
作者:
I. Ohnuma;R. Kainuma;K. Ishida
通讯作者:
I. Ohnuma;R. Kainuma;K. Ishida
影响因子:
6
作者:
Chu, Kunmo;Sohn, Yoonchul;Moon, Changyoul
通讯作者:
Moon, Changyoul
影响因子:
2.1
作者:
S. Pat;Soner Özen;Volkan Şenay;Ş. Korkmaz
通讯作者:
S. Pat;Soner Özen;Volkan Şenay;Ş. Korkmaz
影响因子:
8.4
作者:
H. Ji;Minggang Li;Shu-yi Ma;Mingyu Li
通讯作者:
H. Ji;Minggang Li;Shu-yi Ma;Mingyu Li
影响因子:
2.1
作者:
Amel Laref-;M. Alsagri;S. Laref;S. Luo
通讯作者:
Amel Laref-;M. Alsagri;S. Laref;S. Luo